Carbon Section
OSK was developed as electrical conductive raw material , heat-resistant raw material, lubricant and mechanical parts in the fields of electricity, semiconductor, machinery and precision machinery.Features of OSK
1. F.C. is more than 99%.
2. Superior conductivity and reinforcement
Analysis Value
FC | VN | Ash |
99.30% | 0.5 | 0.2 |
Ch | 粒系 | 累計 | 区間 |
1 | 0.10 | 0.00 | 0.00 |
2 | 0.12 | 0.00 | 0.00 |
3 | 0.14 | 0.00 | 0.00 |
4 | 0.17 | 0.00 | 0.00 |
5 | 0.20 | 0.00 | 0.00 |
6 | 0.23 | 0.00 | 0.00 |
7 | 0.28 | 0.00 | 0.00 |
8 | 0.33 | 0.00 | 0.00 |
9 | 0.39 | 0.00 | 0.00 |
10 | 0.46 | 0.00 | 0.00 |
11 | 0.55 | 0.00 | 0.00 |
12 | 0.65 | 0.00 | 0.00 |
13 | 0.77 | 0.00 | 0.00 |
14 | 0.92 | 0.00 | 0.00 |
15 | 1.09 | 0.00 | 0.00 |
16 | 1.29 | 0.00 | 0.00 |
17 | 1.53 | 0.00 | 0.00 |
18 | 1.81 | 0.00 | 0.00 |
19 | 2.15 | 0.00 | 0.00 |
20 | 2.55 | 0.00 | 0.00 |
21 | 3.02 | 0.00 | 0.00 |
22 | 3.58 | 0.00 | 0.00 |
23 | 4.24 | 0.00 | 0.00 |
24 | 5.03 | 0.00 | 0.00 |
25 | 5.97 | 0.00 | 0.00 |
26 | 7.07 | 0.00 | 0.00 |
27 | 8.39 | 0.00 | 0.00 |
28 | 9.95 | 0.00 | 0.00 |
29 | 11.79 | 0.34 | 0.34 |
30 | 13.98 | 2.31 | 1.97 |
31 | 16.58 | 6.68 | 4.37 |
32 | 19.66 | 14.24 | 7.56 |
33 | 23.31 | 25.37 | 11.13 |
34 | 27.64 | 39.61 | 14.24 |
35 | 32.78 | 55.53 | 15.92 |
36 | 38.86 | 71.04 | 15.51 |
37 | 46.08 | 84.06 | 13.02 |
38 | 54.64 | 93.22 | 9.16 |
39 | 64.79 | 98.29 | 5.07 |
40 | 76.82 | 100.00 | 1.71 |
41 | 91.09 | 100.00 | 0.00 |
42 | 108.01 | 100.00 | 0.00 |
43 | 128.07 | 100.00 | 0.00 |
44 | 151.86 | 100.00 | 0.00 |
45 | 180.07 | 100.00 | 0.00 |
46 | 213.51 | 100.00 | 0.00 |
47 | 253.17 | 100.00 | 0.00 |
48 | 300.19 | 100.00 | 0.00 |
49 | 355.95 | 100.00 | 0.00 |
50 | 422.06 | 100.00 | 0.00 |
51 | 500.45 | 100.00 | 0.00 |
52 | 593.40 | 100.00 | 0.00 |
53 | 703.61 | 100.00 | 0.00 |
54 | 834.27 | 100.00 | 0.00 |
55 | 100.00 | 100.00 | 0.00 |
粒径 μm Grain size 累積 % Accumulation % 区間 % Path %